Jeep Prepares to Recall New Wranglers Over Frame-Weld Defect

Jeep Wranglers are displayed at a dealership in New York City on July 23, 2018.

Photographer: Spencer Platt/Getty Images 

Lock
This article is for subscribers only.

Fiat Chrysler Automobiles NV is preparing to recall about 18,000 Jeep Wranglers because of a faulty weld in the frame of the popular sport utility vehicle that can cause a sudden crash.

The automaker will begin the recall before the end of the year, according to a dealer notice posted Friday on a Wrangler owner forum that was confirmed by the company. Some vehicles have a faulty weld on the front track bar, which keeps the axles centered. That can allow the bar to separate from the frame and interfere with the steering, “which can cause a vehicle crash without prior warning,” according to the notice.